How many of these inexplicable welding defects have you encountered?
2026-11-24
In our daily work, we receive many customer inquiries about welding issues. During the welding process, customers may encounter some inexplicable welding defects, which have different causes. In actual SMT surface mount processing or plug-in soldering, we generally adopt some methods to avoid the occurrence of these soldering defects. So what are the common product failures caused by poor welding? Let me try to give you some simple introductions.
Ideal solder joint Before checking for defects in solder joints, it is best to compare an image of an ideal solder joint.
Figure 1: Ideal solder joint
Ideal solder joints have good surface wettability, meaning that molten solder should spread out on the surface of the welded metal and form a complete, uniform, and continuous solder coating. The correct amount of solder should be sufficient to cover the solder joints without being too much or too little.
Common welding defects 1. Excessive solder (risk of non wetting and bridging)
Common beginners in welding believe that more solder is better, but excessive solder can cause the solder ends and pins of the components to be surrounded by too much solder, or there may be bubbles in the middle of the solder joints, which are characterized by circular and protruding shapes. However, it is difficult to know what actually happened underneath the solder, as there is a possibility that the pins and pads have not been properly wetted. In this way, on the one hand, it will waste solder, and on the other hand, it will increase the risk of bridging formation (i.e. unexpected connection when two solder joints are connected, or causing a short circuit on the circuit board).
So, sufficient solder is enough to thoroughly wet the pins and pads, and more importantly, it is important to control the soldering temperature and time. In addition, pay attention to whether there is enough space between the solder pad and the solder mask layer.
Figure 2: Excessive solder
Figure 3: Excessive solder, unexpected connection forming a bridge
In addition, it is best to prevent the formation of bridging by using the correct lead length. The suitable lead length depends on the size and thickness of the PCB board, as well as the size and quality of the components; In addition, you should use the correct hole size and pad diameter for through-hole parts.
Removing excess solder from the circuit board may be time-consuming.
The use of solder strips (also known as "solder wires") can economically and efficiently remove excess solder.
So how do you choose a tin absorbing tape that meets your project requirements?
You can take a look at this sharing: Choose the appropriate solder suction tape
2. Solder ball
Solder balls are also one of the most common welding defects, usually occurring in wave soldering or reflow soldering. It looks like a small sphere, adhering to the PCB board and the surface of the resist.
There are many reasons for solder balls, mainly including the following two reasons:
When soldering PCB boards, the moisture near the through holes on the PCB board will turn into steam due to heating. If the metal coating on the hole wall is thin or has gaps, water vapor will be removed through the hole wall. If there is solder in the hole, water vapor may squeeze out the solder and produce solder balls on the front of the printed board.
2. The formation of solder balls on the back of the PCB board (in contact with the wave soldering surface) is caused by improper setting of certain process parameters for wave soldering. If the amount of flux applied increases or the preheating temperature is set too low, it may affect the evaporation of components in the flux. When the PCB board enters the peak, excess flux will evaporate at high temperatures, and solder will splash out of the solder bath. The surface of the printed circuit board may produce irregular solder balls.
Figure 3: Solder ball
3. Cold welding
The surface of cold welding appears dull and uneven.
Figure 4: Cold Welding
This is usually due to insufficient heat transfer to the solder joint to completely melt the solder, one reason being that the soldering iron or solder joint itself may not have received enough time to fully heat up, the soldering iron temperature may not have been set high enough to melt the type of solder being used (for example, Chip Quik's RASWLF.031 1OZ lead-free solder has a melting point of 217-220 ° C), or this may be a result of the design of the solder pads and traces themselves. For example, a solder pad is directly connected to the ground plane without considering heat dissipation issues, resulting in the heat dissipation of the solder pad to the ground plane. If you find that stubborn solder joints cannot liquefy, then you need to check if there are any design issues.
Figure 5: RASWLF.031 1OZ lead-free solder for Chip Quik
4. Stele erection
The phenomenon of "erecting a monument" usually occurs on surface mount components, such as resistors or capacitors. Ideally, the solder will adhere to two solder joints during the soldering process and begin to wet. However, if the solder on one solder joint is not completely wet, one side of the component will tilt, causing the resistor or capacitor side to be lifted up from the solder joint like a "tombstone".
Figure 6: The component is lifted up like a tombstone
Some possible reasons for this type of problem:
1. The melting time of solder at both ends of the component is not synchronized or the surface tension is different
2. Solder pad design: The outward extension of the solder pad routing should be within the range specified in the specification book. If it is too short or too long, it is easy to cause the phenomenon of standing a monument.
3. The solder is too thick, and melting the solder will cause the components to float up
4. Temperature curve setting: Stele erection generally occurs at the moment when the solder joint begins to melt, and the slower the heating rate near the melting point, the more beneficial it is to eliminate the phenomenon of stele erection.
5. One solder joint of the component is oxidized or contaminated and cannot be wetted.
Some components may have some flaws themselves, but there may not necessarily be a problem. For details, please refer to this sharing:
Abnormal plating of component pins
5. Poor wetting and virtual soldering
If the solder pads are not fully wetted, the component cannot form a firm connection with the circuit board. Ideally, the solder should achieve 100% wetting with the pads and pins, leaving no gaps or exposed spaces. Insufficient wetting of pins and pads is due to failure to heat the pins and pads, and insufficient time for solder to flow, which may result in virtual soldering.
The reasons for this are mostly contamination of the welding area surface, contamination by solder resist, or the formation of a metal oxide layer on the surface of the joint. To solve this problem, it is necessary to thoroughly clean the circuit board and evenly heat the solder pads and pins.